A doctoral thesis by Plinio Fernandes Borges Silva, a PhD student at Chalmers University of Technology, and a news release dated November 19, disclose a molecular-level mixing process that deposits a graphene oxide (GO) coating on copper powder surfaces via an APTES coupling agent. The process has been scaled from 20-gram small batches to 500-gram batches, with a cumulative 10 kilograms of GO-coated copper powder produced. In pure copper laser powder bed fusion (PBF-LB), the GO coating lowers the powder's laser reflectivity and changes melting behavior: operando X-ray radiography shows shallower, wider keyholes in the melt pool. Validation parts built on commercial EOS production equipment achieved higher relative density and a wider printing window for thin-walled structures. More importantly, GO acts as a sacrificial layer that participates in the reaction, significantly reducing the oxygen content of the final components and improving the wetting and spreading of molten copper. The research was carried out at the CAM2 competence center (funded by VINNOVA) and comprises two core papers. Pure copper printing has long been constrained by high reflectivity and high thermal conductivity; powder surface engineering, rather than changing the alloy composition, offers a third technical route. The 10-kilogram production scale means that coated powder has moved beyond the laboratory gram-level concept and now has a basis for scaling up to industrial applications such as copper components for heat exchangers.