Eplus3D has announced progress in the industrialization of pure copper and copper alloy 3D printing. The company has developed a dedicated high-reflectivity machine and process to solve the problem of unfused porosity in copper printing. Its printed copper parts achieve density above 99.9%, with pure copper conductivity reaching up to 100% IACS and thermal conductivity exceeding 400 W/m·K. The solution enables the fabrication of large solid cross-sections, complex internal channels, and thin-wall structures, and has been applied in scenarios such as rocket engine thrust chambers and heat dissipation components.