🔬 Common Alloy Reference

Standard mechanical properties for the four most common metal 3D printing alloys. Prices are current market lows from our database.

Property Ti-6Al-4V AlSi10Mg 316L Inconel 718
Density4.43 g/cm³2.68 g/cm³7.99 g/cm³8.19 g/cm³
Tensile Strength (UTS)950–1050 MPa320–380 MPa540–620 MPa980–1100 MPa
Yield Strength (0.2%)880–950 MPa200–250 MPa450–520 MPa700–800 MPa
Elongation10–15%4–8%30–45%15–22%
Hardness32–36 HRC95–115 HBW20–25 HRC35–40 HRC
💰 Market Price (USD/kg)$44 – $52$10 – $22$8 – $9$44 – $49
Typical ApplicationsAerospace structural, medical implants, turbine bladesAutomotive heat exchangers, lightweight housingsFood processing, chemical tanks, surgical toolsJet engines, gas turbines, nuclear reactors

Properties from ASTM/AMS standards for as-built LPBF material (heat treated). Prices updated live from our product database.