Patent CN122669314A, applied for by Central Iron and Steel Research Institute Co., Ltd. (publication date September 1, 2026), discloses a high-N, Al-containing 25Cr-type duplex stainless steel powder and a laser powder bed fusion (LPBF) method therefor. The invention aims to address the problems of molten pool disturbance, elemental loss, and increased cracking risk caused by high nitrogen content during LPBF processing of high-nitrogen duplex stainless steels. The powder composition features specific ratios of Cr, Mo, Ni, N, and Al, with the goal of achieving stable fusion and macro-crack-free forming in laser powder bed fusion.