The hot isostatic pressing (HIP) equipment with the world's largest hot zone, independently developed by Sichuan Aviation Industry Chuanxi Machinery, passed pressure test monitoring by the Sichuan Provincial Special Equipment Inspection and Research Institute in Anshun, Guizhou. The equipment features a hot zone diameter of 2400mm and a height of 3500mm, with test pressure reaching 205MPa; data from the entire pressurization, holding, and depressurization process were complete and all indicators were controlled. HIP equipment is key process equipment for powder metallurgy forming and performance enhancement of new materials, covering fields such as nuclear materials, aerospace materials, cemented carbide, superalloys, and semiconductor targets. The project achieved full-process independent controllability.