Dengwei International Trading (Shanghai) Co., Ltd., under its Dengwei Special Steel brand, is promoting its TA0 titanium alloy product line within the Yangtze River Delta specialty alloy supply chain. On October 29, 2026, the company released supply information covering three product forms: spherical titanium powder, cold-rolled titanium strip coil, and open-die forged flanges. The spherical titanium powder has a particle size range of 15–53 μm and an oxygen content controlled below 0.15%, explicitly targeting two high-threshold applications: metal 3D printing and medical implants. Technically, the spherical titanium powder emphasizes high sphericity and compliance with Hall flowability standards, with no hollow particles or impurity inclusions. Printed bodies are free of internal porosity and inclusions, and purity meets the ISO 5832 specification for metallic materials for surgical implants. The printing process window involves high-temperature forming at 1600°C under inert argon protection. The cold-rolled titanium strip coil has a thickness of 0.05–1.0 mm, a width of 100–600 mm, and a coil length of 500–3000 m, making it suitable for roll-to-roll continuous magnetron sputtering coating lines. The open-die forged flanges have an outer diameter of φ200–1000 mm and a thickness of 20–80 mm, with mirror-finished sealing surfaces, intended for high-purity reagent storage tank applications. The three product types correspond respectively to additive manufacturing, flexible optical coating, and fine chemical storage conditions, with the matching relationship between material form and end-use process described in considerable detail. For the metal additive manufacturing supply chain, TA0 spherical titanium powder combines medical-grade purity and 3D printing flowability requirements into a single powder specification. This means that feedstock for personalized implantable devices such as maxillofacial repair scaffolds, porous bone fillers, and cerebrovascular micro-stents now has a clear domestic supply chain option, and powder buyers can use this to verify oxygen content and sphericity against the ISO 5832 specification. Value for powder buyers: ① Prioritize requesting oxygen content test reports and Hall flowability data for the 15–53 μm spherical titanium powder to verify that oxygen content is consistently below 0.15%; ② For medical implant applications, require suppliers to provide an ISO 5832 compliance statement and confirm batch screening records showing no hollow particles; ③ If titanium strip coil or forged flanges are also involved, buyers can leverage Dengwei Special Steel's dual-warehouse stock system to conduct centralized multi-form price negotiations, reducing logistics and inspection costs for cross-category procurement.