Aluminum Alloy Powder CNPC-AlMgMnZr
Aluminum Alloy · CNPC-AlMgMnZr · 20-63 μm、可定制
Price Range / 价格区间
● In Stock
Supplier / 供应商
Unknown Supplier
China
Technical Specifications / 技术规格
Description / 产品描述
[Product Overview] CNPC-AlMgMnZr is a high-strength aluminum alloy powder produced by advanced gas atomization (AMP) and vacuum induction gas atomization (VIGA) processes. The powder exhibits excellent sphericity and flowability, making it ideal for additive manufacturing. [Chemical Composition] - Fe: ≤0.5% - Cu: 9-11% - Si: rr - Al: Bal. [Physical Properties] - D10: 13 μm - D50: 32 μm [Mechanical Properties] - Sintering activity: stable - High flowability: ≥340 s/50g - Tensile strength (heat treated): ff MPa [Applications] Suitable for lightweight applications in aerospace, automotive manufacturing, and other industries.
Compare Similar Products
| Product | Particle Size | Price (USD/kg) | Supplier | Certifications | |
|---|---|---|---|---|---|
| Aluminum Alloy Powder CNPC-AlMgMnZr Current | 20-63 μm、可定制 | $0 – $0 | Unknown Supplier | — | |
| AlSi(5-70) Aluminum-Silicon Alloy Powder for Additive Manufacturing | 20-63um | $10 – $22 | Hunan AoKe New Material Technology Co., Ltd. ✓ | — | Compare → |
| AlSi10Mg Aluminum Alloy Powder for Additive Manufacturing | 20-63μm | $12 – $12 | Inner Mongolia Sunruns New Material Co., Ltd. ✓ | — | Compare → |
| 6061 Aluminum Alloy Powder for Additive Manufacturing | 20-63um | $12 – $15 | Hunan AoKe New Material Technology Co., Ltd. ✓ | — | Compare → |
| 2024 Aluminum Alloy Powder for Additive Manufacturing | 20-63um | $20 – $34 | Hunan AoKe New Material Technology Co., Ltd. ✓ | — | Compare → |
| 7075 Aluminum Alloy Powder for Additive Manufacturing | 15-53um | $26 – $38 | Hunan AoKe New Material Technology Co., Ltd. ✓ | — | Compare → |
📊 Price Trend — Aluminum Alloy
Prices shown are EXW (factory gate) in USD/kg. Data from PowderSight Price Index.