Skip to main content
1 USD = 6.80 CNY | Source: ExchangeRate-API | View Prices →
🔬

2024 Aluminum Base Alloy Powder

Other · 2024 Aluminum Alloy · 参考标准值

Price Range / 价格区间

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
2024 Aluminum Alloy
Particle Size
参考标准值
Process
真空熔炼气雾化制粉

Technical Specifications / 技术规格

Grade: 2024 Aluminum Alloy | PSD: | Process:

Description / 产品描述

2024 Aluminum Base Alloy Powder Suitable for SLM3D