925 Silver Alloy Powder

Other · 925银合金粉末 · 15-53μm

Price Range / 价格区间

$0.00 - $0.00 / per kg

MOQ: 10 kg

Lead Time: 7-14 days

● In Stock

Grade
925银合金粉末
Particle Size
15-53μm
Process
未明确

Technical Specifications / 技术规格

Grade: 925银合金粉末 | Particle Size: 15-53μm | Process: 未明确 | Application: 珠宝与时尚饰品制造、电子与导电材料、医疗与抗菌领域、工业催化与化工

Description / 产品描述

925 Silver Alloy Powder. Suitable for 珠宝与时尚饰品制造、电子与导电材料、医疗与抗菌领域、工业催化与化工.