Jiangsu Mengda New Energy Materials Co., Ltd. has initiated the environmental impact assessment for a '6,500-ton annual metal powder project' located in Nantong, Jiangsu Province. Mengda New Energy is a high-tech enterprise specializing in new energy materials and metal powders. Its parent company's 'Mengda' series metal powders are widely used in cemented carbides, powder metallurgy (PM/MIM), electronic components, diamond tools, and new energy sectors. The company has recently filed several 3D printing-related patents, including 'A Mixing Device Based on Metal Powder 3D Printing' and 'A Treatment Device for Improving Sphericity of 3D Printing Metal Powders.' The advancement of this project will further expand domestic metal powder production capacity, bolstering the supply of upstream materials for additive manufacturing.