Jiangsu Mengda New Energy Materials Co., Ltd. has initiated the environmental impact assessment (EIA) for its "Annual 6,500-ton Metal Powder Project" located in Nantong, Jiangsu Province. The company is a high-tech enterprise specializing in new energy materials and metal powders. Its parent company's "Mengda" series metal powders are widely used in industries such as cemented carbide, powder metallurgy (PM/MIM), electronic components, diamond tools, and new energy. Recently, the company has filed several 3D printing-related patents, including "A Blending Device for Metal Powder 3D Printing" and "A Processing Device for Improving Sphericity of 3D Printing Metal Powders." The project will further expand domestic metal powder production capacity and strengthen the supply of upstream materials for additive manufacturing.