U.S. metal powder manufacturer 6K Additive reported net revenue of $7.1 million for the second quarter of 2026, up 63% year-on-year and 14% quarter-on-quarter. Revenue from the powder business reached $5.0 million, up 25% from $4.0 million in the prior quarter and a 63% increase from $3.1 million in the same period last year. Alloy business revenue was $2.1 million, compared to $1.3 million in the prior year. Repeat orders accounted for over 90% of total revenue. Backlog at quarter-end stood at $11.9 million, up 23% quarter-on-quarter, while new powder orders grew 28% sequentially. The company continues to expand capacity, planning capital investments of $11–12 million in 2026. 6K Additive produces high-performance metal powders from recycled scrap using its proprietary UniMelt® plasma technology. The revenue growth reflects structural demand for localized, sustainable metal powders in the defense and aerospace sectors.