A University of Washington team published a study in Materials (October 29): Using in-situ optical tomography on an EOS M290, they quantified the spatial distribution of spatter during laser powder bed fusion of Ti6Al4V—spatter volume in the upwind region was significantly higher than in the downwind region, gas-atomized powder produced more spatter than plasma-atomized powder, and high-spatter areas were positively correlated with the risk of lack-of-fusion defects.