CoCrMoW Cobalt-Chrome Alloy for Medical Implants

✓ Verified

Cobalt-Chrome · CoCrMoW · 15-45 μm

Price Range / 价格区间

$191.50 - $235.50 / per kg

MOQ: 2 kg

Lead Time: 10-14 days

● In Stock

Grade
CoCrMoW
Particle Size
15-45 μm
Process
EIGA

Supplier / 供应商

P

Peshing Advanced Metals

Jiangsu, China

Verified
ISO 9001 ISO 13485

Technical Specifications / 技术规格

Chemical: Co Bal, Cr 28.0-30.0%, Mo 5.0-6.0%, W 4.0-5.0% | PSD: 15-45 μm | App Density: >=4.2 g/cm³ | UTS: >=1100 MPa | YS: >=650 MPa | Biocompatibility: ISO 10993 certified

Description / 产品描述

Medical-grade CoCrMoW cobalt-chrome alloy powder certified for dental and orthopedic implant applications. Excellent biocompatibility and high wear resistance.