Grade Profile

18Ni300 (1.2709 / MS1): The Highest-Strength AM Steel

Soft as printed, up to 2,000 MPa after ageing — the maraging alloy that builds the world’s strongest molds and tooling.

Published 2026-11-26 · Data: PowderSight supplier catalog & industry sources · ~5 min read
2,000 MPa classAs-built ~1,230 MPa UTS; a 490 °C ageing cycle develops up to 1,800-2,000 MPa — the strongest common AM steel.
Print soft, age hardLow-carbon martensite machines easily as-built, then age-hardens with minimal distortion.
Tooling + moreInjection inserts, punches, aerospace tooling — anywhere ultimate hardness meets tight tolerances.

1 · Why 18Ni300

18Ni300 maraging steel (1.2709, MS1) hardens not by carbon but by intermetallic precipitation of Ni-Co-Mo-Ti phases. The result is a steel that prints soft and machinable, then ages to 1,800-2,000 MPa with almost no distortion — the combination that makes it the strongest practical AM steel.

For tooling it solves the H13 dilemma: machined inserts made of conventional steel cannot carry internal cooling and extreme hardness together; printed 18Ni300 inserts do both. Punches, dies, gripper fingers and aerospace tooling all run on the same logic.

2 · Process & Heat Treatment

Standard supply is 15-45 µm and 15-53 µm VIGA powder. The standard ageing is ~490 °C for 3-6 hours after printing — no quench needed, minimal distortion, and the hardness lands reproducibly in the 50-54 HRC band.

Age before final machining. Machine in the as-built state, then age — the low-carbon matrix cuts like butter pre-ageing.
Watch Ti and Mo. The ageing response depends on Ti/Mo content — verify measured chemistry per DIN 1.2709.

3 · Applications & Market Signals

Demand concentrates in injection-mold inserts (high-cavitation, glass-filled resins), high-strength tooling (punches, dies) and aerospace tooling where weight and strength both count.

Glass-filled resins drive inserts. Abrasive compounds eat H13 surfaces; 18Ni300’s aged hardness extends insert life.
Conformal cooling + maraging. The strongest cooling-channel inserts combine 18Ni300’s hardness with printed internal channels.

4 · Four-Point Buying Checklist

1 · Chemistry per DIN 1.2709 / AMS 6514. Measured Ni/Co/Mo/Ti values — they set the ageing response.
2 · PSD. 15-45 µm for fine features, 15-53 µm general purpose.
3 · Cleanliness. O/N content and inclusion rating — fatigue-critical tooling needs clean steel.
4 · Ageing validation. Run a test coupon through your ageing cycle and verify hardness before volume.

FAQ · 18Ni300 (1.2709 / MS1)

What is the heat treatment for 18Ni300?

Simple ageing: ~490 °C for 3-6 hours after printing. No quench, minimal distortion, hardness lands at 50-54 HRC. Machine in the as-built state first.

How strong is printed 18Ni300?

As-built LPBF parts reach ~1,230 MPa UTS; after ageing the alloy develops up to 1,800-2,000 MPa — the highest strength of any common AM steel.

18Ni300 vs H13 for tooling — which one?

H13 for hot-work and die-casting (thermal fatigue resistance); 18Ni300 for maximum hardness and wear in injection molds and cold-work tooling.

Source 18Ni300 with confidence Post your requirement with full specification — verified suppliers respond within 24 hours. The more complete your spec, the faster the quotes.
Post a 18Ni300 Requirement → Suppliers →