1 · Why Ti-6Al-4V ELI
Ti-6Al-4V ELI (Grade 23) is the ultra-low-interstitial variant of Grade 5: oxygen capped at 0.13% and iron at 0.25%. Those two limits transform fracture toughness and fatigue crack growth — the properties that decide whether an implant survives 30 years of load cycles or an airframe part flies.
Every extra 100 ppm of oxygen trades ductility for strength; ELI chemistry deliberately gives that trade away, which is why medical implants (ASTM F136) and aerospace fracture-critical parts specify Grade 23 rather than Grade 5. The powder route matters: EIGA keeps oxygen low through inert-gas handling from melt to can.
2 · Process & Certification
Standard supply is 15-45 µm and 15-53 µm EIGA-atomized powder. Implant-grade lots ship with chemistry per ASTM F136 / F3001, full PSD, and oxygen/nitrogen certificates — the paperwork is part of the product.
3 · Applications & Market Signals
The demand split: medical implants (spinal cages, acetabular cups, trauma plates — regulated, sticky), and aerospace fracture-critical parts (brackets, housings under flight-critical loads).
4 · Four-Point Buying Checklist
FAQ · Ti-6Al-4V ELI (Grade 23)
Chemistry: ELI caps oxygen at 0.13% and iron at 0.25%, trading a little strength for significantly better fracture toughness and fatigue life — the reason implants and fracture-critical parts specify Grade 23.
15-45 µm for fine implant geometry, 15-53 µm for larger components. EBM uses 45-106 µm. State the device type in your RFQ.
No — the process window is essentially the same; the extra discipline is in powder certification and oxygen control, not machine parameters.
Data notes: based on PowderSight supplier catalog records and public industry sources. This article is informational and does not constitute a price quote.