PowderSight Research · Grade Profile EN HomeChinese Version
Grade Profile

TA15: China’s High-Temperature Titanium Workhorse

The near-alpha alloy that keeps strength to 500°C — engine casings, airframes and the hottest structural jobs in Chinese aerospace.

Published 2026-11-26 · Data: PowderSight supplier catalog & industry sources · ~5 min read
500 °C serviceA near-alpha composition (Ti-6.5Al-2Zr-1Mo-1V) that holds strength where Ti-6Al-4V starts to fade.
Aerospace pedigreeThe standard Chinese airframe and engine structural titanium — Russian VT20 equivalent with deep domestic supply.
Thin-wall friendlyPrints 15-53 µm (LPBF) and 45-106 µm (EBM) with good weldability for laser repair.

1 · Why TA15

TA15 (Ti-6.5Al-2Zr-1Mo-1V) is a near-alpha titanium alloy — alpha-stabilized by Al with just enough Zr, Mo and V to retain hot strength without the beta-rich brittleness. The result is a structural alloy that serves continuously at up to 500 °C, above the comfortable ceiling of Ti-6Al-4V.

In Chinese aerospace it is the default material for engine casings, hot airframe sections and high-temperature brackets; the Russian designation VT20 marks the same alloy family. AM adoption is growing through laser repair and cladding of forged TA15 parts plus new LPBF structural prints.

2 · Process & Particle Size

LPBF runs 15-53 µm gas-atomized powder; EBM uses 45-106 µm. Near-alpha alloys are less hot-crack sensitive than α+β grades, but oxygen pickup is the controlling variable: every 100 ppm of oxygen measurably shifts ductility and fatigue.

Watch the alpha case. EBM and HIP runs at high temperature — specify the vacuum level and check surface hardness after post-processing.
Zirconium homogenization. Zr segregates slowly; demand chemistry uniformity data across the lot.

3 · Applications & Market Signals

Demand concentrates in aerospace structural parts (brackets, casings, hot skins) and high-temperature components for engines; laser-cladding repair of forged TA15 is the fastest-growing niche.

Repair beats replace. Blisk and casing repair via powder-fed cladding turns TA15 powder into a consumable for MRO — recurring small-lot demand.
Hypersonic interest. Hot-structure R&D programs are screening near-alpha alloys, pulling premium TA15 lots with tight oxygen control.

4 · Four-Point Buying Checklist

1 · Chemistry per GB/T 3620. Confirm Al/Zr/Mo/V measured values and oxygen ≤ 1,300 ppm (or your spec).
2 · PSD by process. 15-53 µm for LPBF, 45-106 µm for EBM — do not mix.
3 · Powder reuse data. Near-alpha powder sieves and reuses well; ask the supplier for reuse-cycle data.
4 · Heat treatment route. Agree the post-print anneal (typically 700-850 °C) before ordering.

FAQ · TA15

What is TA15 titanium used for?

High-temperature aerospace structures: engine casings, airframe hot sections and brackets serving up to 500 °C, plus laser-cladding repair of forged TA15 parts.

How does TA15 compare to Ti-6Al-4V?

TA15 is near-alpha (better hot strength, ~500 °C service) while Ti-6Al-4V is α+β (better room-temperature ductility). Choose TA15 when the part sees sustained heat.

What particle size should I specify for TA15?

15-53 µm for LPBF, 45-106 µm for EBM, and coarser cuts for laser cladding. State your machine and process in the RFQ.

Source TA15 with confidence Post your requirement with full specification — verified suppliers respond within 24 hours. The more complete your spec, the faster the quotes.
Post a TA15 Requirement → Suppliers →

Data notes: based on PowderSight supplier catalog records and public industry sources. This article is informational and does not constitute a price quote.