1 · Why Inconel 625
Inconel 625 (UNS N06625, GH3625 in China) is a nickel-chromium-molybdenum superalloy that delivers corrosion resistance first and strength second. The Mo and Nb additions buy pitting and crevice resistance in seawater, reducing and oxidizing acids, and hot chlorine-containing gas streams — the exact environments that destroy stainless steels.
Because 625 is solid-solution strengthened rather than precipitation-hardened, printed parts need no ageing treatment: a stress-relief anneal is enough. That shortens the production chain and removes a whole class of heat-treatment distortion problems, which is why 625 is the default superalloy for chemical processing and marine AM parts.
2 · Process & Particle Size
LPBF commonly uses 15-45 µm or 15-53 µm gas-atomized powder; DED and blown-powder cladding use 45-106 µm. The wide window reflects the grade’s tolerance — but niobium segregation is the classic trap: Nb tends to concentrate in coarse particles, so insist on a full PSD report and homogeneous chemistry.
3 · Applications & Market Signals
Platform demand concentrates in three zones: marine components (pump impellers, valve bodies, propellers), chemical processing (reactor internals, scrubbers) and aerospace exhaust systems.
4 · Four-Point Buying Checklist
FAQ · Inconel 625 (GH3625)
15-45 µm for fine-detail LPBF parts, 15-53 µm as the general-purpose cut, 45-106 µm for DED and laser cladding. Mention your machine model in the RFQ so suppliers recommend the right cut.
Only stress relief. Unlike precipitation-hardened grades such as Inconel 718, 625 is solid-solution strengthened and as-built parts are service-ready after annealing.
718 is precipitation-hardened (aged to higher strength, hot-crack sensitive); 625 is corrosion-first and prints with a wider process window. Pick 625 for aggressive environments, 718 for high-temperature strength.
Data notes: based on PowderSight supplier catalog records and public industry sources. This article is informational and does not constitute a price quote.