PowderSight Research · Grade Profile EN HomeChinese Version
Grade Profile

H13: The Conformal-Cooling Tool Steel

Print cooling channels that machining cannot reach — the powder that turned injection molding into an AM business case.

Published 2026-11-26 · Data: PowderSight supplier catalog & industry sources · ~5 min read
The mold gradeThe most popular tool-steel powder in AM — injection-mold inserts and die-casting cores with internal cooling channels.
Strong as-built~1,890 MPa UTS as-built, then quench & temper to a serviceable 48-52 HRC.
Proven economicsConformal cooling typically cuts cycle time 20-40% — the AM business case that pays for itself.

1 · Why H13

H13 (1.2344, SKD61) is the hot-work tool steel that dominates metal AM tooling. Its Cr-Mo-V composition survives hot plastic contact while holding dimensional stability — and AM unlocks the geometry that machining cannot: conformal cooling channels that follow the cavity wall and pull heat out evenly.

The business case is direct: cycle time drops of 20-40% on hard-to-cool geometries, scrap falls with even shrinkage, and the insert pays for itself in months. That is why H13 inserts with conformal cooling are the entry product for most AM service bureaus.

2 · Process & Heat Treatment

Standard supply is 15-53 µm gas-atomized powder. As-built LPBF H13 is a hard martensitic structure (≈560 HV) that must be quenched and tempered to 48-52 HRC for service — direct-from-plate use risks brittleness.

Stress relief early. Cut the part off the plate carefully and stress-relieve before machining; H13 as-built carries high residual stress.
Temper to the application. Die-casting cores run softer (44-46 HRC) for thermal fatigue resistance; injection inserts harder (48-52 HRC).

3 · Applications & Market Signals

The volume stack: injection molds with conformal cooling (largest), die-casting inserts (thermal fatigue is the fight), and hot forging tools.

Bureaus standardize on H13. It is the reference material for mold AM — supply is deep and price competition is real.
Hybrid tooling grows. Printing only the insert onto a conventional mold base squeezes the AM cost further and widens adoption.

4 · Four-Point Buying Checklist

1 · Chemistry per ASTM A681 / DIN 1.2344. C, Cr, Mo, V measured values on the lot certificate.
2 · PSD. 15-53 µm standard; finer cuts only if the channel cross-section demands it.
3 · Inclusion control. Tool steel lives and dies by cleanliness — ask for O/N content and inclusion rating.
4 · Heat-treatment recipe. Confirm quench & temper parameters with the supplier before volume.

FAQ · H13

What heat treatment does printed H13 need?

Quench and temper: solutionize ~1,020 °C, quench, then temper to 48-52 HRC for injection molding or 44-46 HRC for die-casting. Stress relief after printing is mandatory.

Why use AM for H13 instead of machining?

Conformal cooling channels that follow the cavity geometry — impossible to drill — typically cut cycle time 20-40% and reduce scrap from uneven shrinkage.

What particle size should I use for H13 mold inserts?

15-53 µm gas-atomized is the standard. Channel widths above ~0.8 mm print reliably at this cut.

Source H13 with confidence Post your requirement with full specification — verified suppliers respond within 24 hours. The more complete your spec, the faster the quotes.
Post a H13 Requirement → Suppliers →

Data notes: based on PowderSight supplier catalog records and public industry sources. This article is informational and does not constitute a price quote.