1 · Why CoCrMo
CoCrMo is the standard cobalt-chromium alloy of medical AM: hip and knee joints, dental crowns and bridges, and increasingly wear-critical industrial parts. The Cr gives corrosion resistance and the Mo strengthens the solid solution — together they produce an alloy that outlasts stainless steels in articulating contact.
In AM, CoCrMo has effectively replaced investment casting in dental and orthopedic workflows: LPBF prints patient-specific geometry directly from scan data, and the mechanicals (≈1,150 MPa UTS, ~32% elongation) clear cast-equivalent requirements with margin.
2 · Process & Certification
Medical-grade lots are gas-atomized at 15-45 µm or 15-53 µm with carbon controlled ≤ 0.14% for ASTM F75 / ISO 5832-4 conformance. Dental labs typically run 15-45 µm for surface finish; orthopedic parts favor 15-53 µm for productivity.
3 · Applications & Market Signals
The volume split: dental (crowns, bridges, frameworks — high mix, fast turnaround), orthopedic implants (hips, knees — regulated, slow to qualify but sticky), and wear parts (valves, nozzles — no medical file needed, fastest entry).
4 · Four-Point Buying Checklist
FAQ · CoCrMo (ASTM F75)
15-45 µm is the standard for dental LPBF — fine enough for marginal fit, coarse enough to flow well. Orthopedic parts typically run 15-53 µm.
Chemistry per ASTM F75 / ISO 5832-4 with carbon ≤ 0.14%, full PSD and oxygen/nitrogen reports, and batch traceability for your device file. State your regulatory market (FDA/CE/NMPA) in the RFQ.
Yes — LPBF CoCrMo meets or exceeds cast F75 mechanicals with higher design freedom, which is why dental and orthopedic AM have largely replaced casting for patient-specific parts.
Data notes: based on PowderSight supplier catalog records and public industry sources. This article is informational and does not constitute a price quote.